  • < Why does AE-VML > is it less likely...

    This is because it has a web tapered specification that thickens the thickness of core from the cutting edge to the shank. It is even more rigid than convent... 詳細表示

    • No:17959
    • Publication Date:2025/09/05 11:11
    • Updated Date:2026/01/16 14:58
  • Coverage of AE-VMFE for deep side mil...

    The AE-VMFE supports up to a depth of 8D (8 times the diameter of the tool). ・ Click here for the AE-VM series catalog 詳細表示

    • No:18128
    • Publication Date:2025/09/05 11:11
    • Updated Date:2025/10/17 13:45
  • Can AE-MS-H regrinding ?

    Can AE-MS-H regrinding ? regrinding is possible. In order to ensure performance, recoating is also recommended. If you are considering recoating and... 詳細表示

    • No:18084
    • Publication Date:2025/09/05 11:11
    • Updated Date:2025/09/30 14:34
  • What is the good DUROREY coating appl...

    What is the good DUROREY coating applied to end mills for high-hardness steel? The DUROREY coating consists of an ultra-heat-resistant layer containing SiC ... 詳細表示

    • No:18025
    • Publication Date:2025/09/05 11:11
    • Updated Date:2025/11/11 15:57
  • A end mill series that can be used fo...

    In addition to a wide range of materials such as S50C, SS400, SUS, and aluminum, the AE-VM series is recommended for end mills that can handle various proces... 詳細表示