Results:10 ,Showing: 1 - 10
What is work hardening of stainless s...
Mechanism of work hardening For example, a brand new cushion is fluffy. However, if you use it for a long time, the cotton will be compressed and become ha... 詳細表示
Is high-speed tapping of stainless st...
Due to chip control and work hardening issues, high-speed tapping is not recommended. 詳細表示
What kind of stainless steel is gener...
Austenitic such as SUS304, ferritic such as SUS405 having strong magnetism, martensitic such as SUS420 that can be heat-treated used in medical instruments ... 詳細表示
Why does tapping on SUS have a short ...
Work hardening of the pilot hole is the cause of short tap life.By reviewing the drilling method(conditions),we aim to extend the life of the tap! Stain... 詳細表示
Which types of stainless steel are th...
Here are some representative examples: SUS304 Austenitic stainless steel. Prone to work hardening and welding adhesion. High cutting resistance and shorter... 詳細表示
Is there a tap for insert screws that...
The A-SFT HL is also compatible with stainless steel. In addition, it can be used for a wide range of workpiece materials such as SS materials, carbon ste... 詳細表示
There are equivalence tables for stainless steel based on various standards: JIS (Japan), ISO 15510 (International), EN (Europe), UNS/AISI (USA), and GB (Chi... 詳細表示
What are the recommended end mills fo...
When used in a machining center, it is recommended to use a helix angle that is stronger than the standard 30° twist. For carbide end mills, we have the AE-... 詳細表示
What is the Pilot hole diameter of st...
For stainless steel, where chips tend to stretch and cutting heat tends to accumulate, managing the maximum diameter at actual size within the standard will ... 詳細表示
How much effective thread length can ...
For ordinary SUS Tap , both spiral fluted tap and spiral pointed tap are for depths up to 1.5~2 times the thread diameter. If it is longer than that, we rec... 詳細表示
Results:10 ,Showing: 1 - 10